During the welding process, a high level of ambient hydrogen can permeate into a material. If this hydrogen remains in the material, it can lead to blistering, loss of ductility and ultimately hydrogen induced cracking (HIC).
Immediately heating material after welding for a prescribed amount of time, based on material thickness, reduces the risk of HIC. This PWHT allows hydrogen to diffuse out of the welded area to prevent HIC.